Welcome: Shenzhen Zhuolida Electronics Co.TD
Language: Chinese ∷  English
Your location: Home > News > Company new

Company new

Electroformed Batch Consistency Acceptance: Sampling Criteria from First Article to Production Lot

electroformed batch consistency acceptance

Electroformed batch consistency acceptance answers whether every later lot still sits on the first article line — not whether this lot is usable. The practice is concrete: incoming inspection draws pieces at the agreed ratio, stabilises them at 23±2 °C, then scans hole position, measures hole size and checks thickness under a vision system, setting the readings beside the first article baseline. First article approval asks whether the process can produce the part at all. Batch acceptance asks whether each lot still holds the same level. Signing one for the other costs either a full inspection later or a chain of concessions nobody stops.

Three deviations dominate the floor. A first article passes, then the lot moves to another bath position and the hole array shifts 3 μm overall; every single piece sits inside tolerance, yet the part fails once loaded on the fixture. Sampling reads only the centre of the sheet, nobody touches the outer 2 mm band, and that band is exactly where thickness runs thinnest. Third, the threshold exists only as a verbal 'anything within ±10 μm is fine' while the drawing says ±7 μm, so a return turns into two competing stories. That class of dispute makes up most quality arguments, and nearly all of it comes from numbers never being written into the clause.

Parameter Window

• Sampling ratio: 20% for lots up to 50 pieces, 10% and no fewer than 8 pieces for 51–200, 5% as the starting point above 200, all written into the acceptance agreement.

• Mandatory items: hole position ±7 μm, hole size ±3 μm, thickness 15–200 μm. Drop any one and an electroformed batch consistency acceptance no longer stands.

• Decision thresholds: a single out-of-tolerance value fails the piece; a lot passes only at mean shift ≤2 μm with Cpk ≥1.33.

• Environment: 23±2 °C, 45–60% RH, at least 2 h stabilisation in the metrology room before measuring, so thermal expansion is taken out of the reading first.

• Gauge repeatability: three re-measures at the same point, spread ≤1 μm, otherwise change instruments — never read gauge noise as lot variation.

• Tightened inspection trigger: mean hole position drift beyond ±3 μm doubles the sampling ratio, returning to normal only after 3 consecutive stable lots.

Manufacturing Process (8 Steps)

1. Freeze the first article baseline — sign off the report together with the full hole map and thickness map; every later comparison refers to it.

2. Finalise the sampling plan — lot size, AQL, sample count, inspection items, signatory on one sheet, stamped by both sides, no verbal terms left over.

3. Reconcile lot and bath position — check bath number and deposition window on the traveller; lots mixed across baths are separated and judged on their own.

4. Dimensional sampling — vision system for hole position and size, snap gauge for thickness, with separate points taken in the outer 2 mm band.

5. Appearance and function — visual check for burrs and warp; stencils also get tension measured at 10–55 N, anything below the lower limit flagged separately.

6. Data comparison — compute the gap between sample mean and first article baseline, and the within-lot spread, as two separate figures.

7. Disposition — conforming lots released with a lot number; deviations routed to one of three paths: piece rework, full lot inspection, or scrap.

8. Record archiving — raw readings, instrument IDs and signatory filed, traceable by lot number back to bath run.

Core Advantages

1. The sampling sheet travels with the lot: how many pieces, which ones, drawn by whom, all on one page, so an electroformed batch consistency acceptance never relies on memory.

2. Two decision layers: single values govern the piece, mean and Cpk govern the lot. One good piece never stands in for two hundred.

3. Comparison runs against the first article baseline on the same instrument, same temperature, same point rules — only then do the numbers line up.

4. The outer band gets its own points, so the thin rim is no longer averaged away.

5. The tightening rule is fixed in advance: drift beyond ±3 μm doubles the sample automatically, without waiting for the buyer to notice.

6. Three disposition paths with a named signatory each — rework, full inspection, scrap — so a return does not reopen the question of responsibility.

Typical Applications

• Precision stencil lots — sampled per 15–200 μm thickness band, each band judged separately.

• Electroformed screen — roundness ±0.002 mm, sampled hole by hole on the vision system.

• Encoder disc lots — track width 50 μm±0.5 μm, a 1 μm excess sends the whole lot back for re-measurement.

• Aperture plate — rib width 20 μm, a broken rib scraps the piece and stays out of lot statistics.

• Ball placement stencil — pitch ±7 μm overall, sampled together with through-hole rate at 30 μm minimum apertures.

• Micro-hole mesh — hole tolerance ±3 μm, 5% sampled with a floor of 10 pieces.

Design and Selection Notes

1. Define 'consistent' first: against the first article or against the drawing nominal. The two baselines yield different verdicts on the same data.

2. Put a number on the sampling ratio. 'Sample as appropriate' is not a clause; AQL and sample size each need their own line.

3. Rank inspection items by function — hole position and size are critical, appearance is secondary, and mixing them on one sheet invites omissions.

4. Every threshold needs an escape route. Single value over, lot mean over, Cpk short — three different paths, not one.

5. Write environment and instrument into the agreement: 23±2 °C against a 20 °C shop floor can differ by around 1 μm.

6. Fix re-measurement count and timing — once at shipment, once at 3 months, once at 6 months — otherwise long-term drift stays invisible.

7. Separate the signatories: process engineering signs first article approval, quality signs batch acceptance, and the two responsibilities do not overlap.

An electroformed batch consistency acceptance is not a certificate; it is a sampling account anyone can recompute. How many pieces, which items, what happens when a value runs over — write those three down and both sides can reconcile. The boundary deserves saying plainly: sampling lowers risk, it is not full inspection, and it is no guarantee on every piece. If 2 of 30 sampled pieces exceed ±7 μm on hole position, the lot goes back for full inspection rather than a larger sample to smooth it over; the ratio only returns to normal after 3 consecutive stable lots. Hold that line and later lots have something to be consistent with.

CATEGORIES

CONTACT US

Contact:赖先生

Phone:+86 18938693450

Tel:0755-2708-8292

Email:yw9@zldsmt.com

Add:深圳市宝安区福永镇新和村福园一路华发工业园A3栋

Scan the qr codeclose
the qr code