The entry chamfer of electroformed micro-hole mesh covers one small stretch only: in the section running from the entry face down 10% of the material thickness, is the mouth a square cut edge, or does it carry an R or a small 45° bevel. The middle of the hole belongs to sidewall profile, the aspect ratio belongs to the forming process, and neither sits in this account. The measuring section is fixed first — saw along the hole axis, take the band from the entry face to 10% of thickness, read the contour on the vision system and the radius on the confocal, three repeats per hole with the median kept. Which face carries the chamfer has to be on the drawing; when both do, measure them apart rather than letting one stand for the other.
Three deviations dominate on the floor. A customer re-tests flow on our sample and reads 12% under nominal; opened up, our entry is square while the sample was rounded, and neither drawing said a word. Second, the chamfer runs too far, the mouth becomes a bell, the lip is left 8 μm thick and collapses under clamping — flow rises, strength does not. Third, a burr at the mouth holds liquid, bubbles will not clear, and flow on the same sheet falls 6% inside ten minutes. None of the three is about aperture size; all three are entry geometry. One more is easily missed: the two faces of a sheet get different chamfers, so flipping it in assembly makes a new batch, and orientation belongs on the drawing.
Parameter Window
• Inlet radius R 3–10 μm, or a 45° ±5° chamfer 2–15 μm wide
• Penetration depth ≤15% of thickness, so 15 μm at most on 100 μm stock; deeper is a bell mouth
• Aperture 30–200 μm at ±3 μm, entry diameter growth after chamfering ≤4 μm
• Thickness 20–100 μm, chamfer face Ra ≤0.2 μm, no roll-over and no burr
• Discharge coefficient Cd 0.78–0.82 against 0.62 for a square entry, at 5–20 kPa
• Nine holes sampled in a 3×3 grid, flow spread ≤5%, single hole within 8% of the median
Manufacturing Process (8 Steps)
1. Preparation — substrate cleaned, conductive layer even, particles held below 25 μm.
2. Electroforming — 1–4 A/dm², with a shield plate trimming current at the hole rims so they do not build up.
3. Thickness control — ground to 20–100 μm, spread within one sheet ≤5 μm, which the chamfer depth is measured against.
4. Stripping — the electroform is peeled off the mandrel, entry face up, never stacked.
5. Entry chamfer — electrolytic, 3–6 V for 20–60 s, depth checked as it goes.
6. Deburring — a short light polish carries off the 1–2 μm tips without opening the radius further.
7. Cleaning — ultrasonic in deionised water, residue flushed from the holes, no drying marks on the entry face.
8. Flow calibration — deionised water at 23±2°C, 5–20 kPa, all nine holes through the meter one by one.
Core Advantages
1. One fixed section: anything below 10% of thickness is out of scope, which removes half the argument.
2. Radius and bevel both verify, with R value, angle and width read as three separate numbers.
3. Depth is capped against the bell mouth, because a lip with thickness left in it is a lip that survives clamping.
4. Flow and geometry reconciled per batch, so an odd Cd goes straight back to inlet radius for a cause.
5. Nine holes cover centre and four corners; a sheet with shallow chamfers at the edges has nowhere to hide, and shift differences show up on one table.
6. Calibration runs on deionised water at fixed temperature and pressure, so a change of shift or operator still compares.
Typical Applications
• Filter mesh for inkjet print heads
• Micro-hole mesh for medical nebulisers
• Pre-filter screens ahead of fuel injectors
• Mist-generating plates in humidifiers
• Restrictor mesh in air-bearing pads
• Flow-limiting discs in chromatography
Design and Selection Notes
1. Put entry geometry on the drawing; an aperture callout with no R guarantees two suppliers who cannot agree. State the chamfered face as well.
2. A larger radius is not automatically better — past R 10 μm Cd climbs slowly while the lip loses strength quickly.
3. Be careful with big chamfers on thin stock: 10 μm on 30 μm material is already a third of the thickness.
4. If flow on the entry chamfer of electroformed micro-hole mesh reads 8% under the sample, re-check inlet radius and differential pressure before touching aperture size.
5. Watch the bath, not just the clock; an aged electrolyte gives roughly 2 μm less R for the same time.
6. Quote the pressure with the flow, since Cd differs by 0.03 between 5 kPa and 20 kPa and the report has to say which.
7. Sheets with entry burr go to rework, which deburring can save; a bell mouth is scrap.
On the bench this is one section image and one flow meter. The inspector sets the sheet in the fixture, brings the differential to 10 kPa and reads nine holes one at a time: median 12.4 mL/min with a worst deviation of 4.1%, a pass. One hole is then sectioned — inlet R 6.8 μm, penetration 9 μm on 60 μm stock, which is 15%, right at the ceiling. Another batch reads R 2.1 μm only and flow 11% under the sample, Cd at 0.68; 30 s back in the electrolytic bath brings it to R 5.4 μm and Cd 0.79, released as rework. There is a boundary here: deeper is not smoother, since past 15% of thickness flow gains another 2% while the lip loses a fifth of its thickness and gives way under clamping or back-flushing. If a customer supplies aperture and open area alone, ask for four more items — inlet R or chamfer angle, a depth ceiling, a Cd band and the calibration pressure — or acceptance turns into two monologues. For inkjet and nebuliser orders, a nine-hole flow sheet is worth far more than the words 'flow OK'. Back-flushing adds about 0.5 μm to the chamfer, so re-test after cleaning. What ships is a section plus flow record: inlet R 3–10 μm, penetration ≤15% of thickness, Cd 0.78–0.82.