An encoder code disc is a thin round sheet carrying equally spaced tracks and lines; the optical head reads track transitions to derive angle. In qingdao encoder code disc electroforming, nickel is deposited onto a patterned mandrel, grown to thickness, stripped as one piece, then cleaned and given a low-temperature anneal. Indexing accuracy consistency means the angular pitch of every line around the circle lands in the same band. The line edge decides how sharp the head's transition is. The shop measures track width on a vision system, checks sheet thickness with a flash system, and samples angles on an indexing table. A little burr on an edge makes the signal jitter, so it has to be caught before the disc is mounted. The head runs on a simple on-off logic: a blunt edge causes more trouble than an angular error and takes longer to trace.
Three faults show up in rework. One, a stretch of track comes out 1.2 μm narrower than the nominal 50 μm and the head drops pulses in that sector. Two, edges grow burrs — visible under the microscope as nickel nodules — and the signal transition blunts. Three, mean angle across the sheet passes while a step in accumulated deviation appears every few dozen lines, traced to misalignment at an exposure stitching segment. These are the costliest failures in qingdao encoder code disc electroforming. On the line they are called poor index consistency, and rework seldom saves the disc; it is scrapped and run again. A skewed zero mark shifts the whole reading and is easily mistaken for an indexing fault.
Parameter Window
• Track width 50 μm ± 0.5 μm, sampled at 12 evenly spaced points around the circle, never at one spot; positions go into the report.
• Aperture rib line width 20 μm, edges measured on the vision system, burr height held within 2 μm and the transition kept sharp.
• LDI resolution 8 μm/8 μm, double-side alignment ± 5 μm, maximum substrate 610 × 660 mm; larger formats are quoted separately.
• Nickel layer thickness in 15–200 μm bands, 30–60 μm the common band, sheet deviation ± 3 μm so the disc seats flat.
• Current density 1–4 A/dm², bath at 23 ± 2 °C, build in stages so the rim does not grow thick first; ramp between stages.
• Nickel alloy hardness 450–550 HV, four radii measured after low-temperature annealing; a 30 HV drift sends the bath back for recheck and the heat number is logged.
Manufacturing Process (8 Steps)
1. Drawing review — check track count, indexing angle and rib width, confirm head type and light direction, and fix the zero mark.
2. Mandrel pre-treatment — make conductive, degrease and activate; measure base roughness first and build up a thin conductive layer.
3. Lamination and LDI — expose the full circle of tracks at 8 μm/8 μm resolution and ± 5 μm double-side alignment, flagging stitching segments.
4. Development — control concentration and time so no residue clings to the line edges; the 20 μm rib width is set here and the time logged.
5. Electroforming — current density 1–4 A/dm² and bath at 23 ± 2 °C, built in stages with mid-run thickness checks.
6. Release and cleaning — peel the nickel disc off the mandrel, strip residue and dry, taking care with the thin ribs at the edge.
7. Low-temperature anneal — relieve stress, record temperature by heat number, then check hardness at 450–550 HV and re-measure warpage.
8. Recheck — vision system measures tracks and line edges, indexing table samples the full circle, and the record is filed; out-of-tolerance discs are sealed.
Core Advantages
• The full circle is exposed in one pass instead of stitching, so one source of accumulated deviation disappears and cross-checking is simpler.
• Line edges are logged on their own, with vision images travelling in the report so the head maker can verify and disputes stay short.
• Track width is sampled at 12 points and must sit inside 50 μm ± 0.5 μm; no single-point mean is handed over.
• Layer thickness is produced in bands; the 30–60 μm band holds ± 3 μm, so the disc seats flat and balancing is easier.
• Local discussion in Qingdao means the indexing angle notation is agreed face to face, cutting revision rounds.
• Faster exposure is not always better: a little residue left behind blurs a 20 μm rib first, so redoing development is cheaper than scrapping.
Typical Applications
• Incremental encoder discs, track 50 μm ± 0.5 μm, stable head pulses with few dropped counts.
• Motor encoder discs at 450–550 HV that hold shape at speed, thickness reported at nine points.
• Aperture discs with 20 μm ribs, clean edges and a steep transition for a better signal-to-noise ratio.
• Master discs for indexing-table calibration, with full-circle angular records traceable to the sampling date.
• Robot joint discs in the 30–60 μm band, ± 3 μm held lot to lot.
• Trial parts for equipment customers in and around Qingdao, supplied with an indexing recheck sheet and no blanket grade promise.
Design and Selection Notes
• Fix the indexing angle from the drawing and give track count and zero mark with it; do not leave the shop to guess.
• Track width 50 μm ± 0.5 μm is a measured band; if a stretch drifts past 50.5 μm, go back to exposure and development.
• Rib widths below 20 μm need review — edge quality falls as the depth-to-width ratio climbs and the head transition blunts.
• If accumulated index deviation exceeds the drawing value, return to the stitching alignment record rather than compensating the angle on paper.
• Choose the 30–60 μm band; stock past 200 μm is outside the usual range for electroformed discs.
• Harder nickel is not always better: above 550 HV the anneal is short and stored stress makes the disc warp.
• Indexing accuracy follows the drawing and measurement, with no blanket grade promised; qingdao encoder code disc electroforming issues a recheck sheet per lot.
Delivered on the line, qingdao encoder code disc electroforming sells not a grade on a datasheet but a record every line around the circle can be rechecked against. Read the track count and zero mark from the drawing first, then rib width and edge, then put the sample on the vision system and indexing table. Any segment out on angle is sorted: rework what can be saved, scrap what cannot. For customers in and around Qingdao the report states the 12 sampling positions and the judgement rule. Indexing accuracy follows the drawing and measurement, with no blanket grade promised; discs with burr edges are held back with a section sample and never mixed into a passing lot.