Tianjin electroformed mask plate processing makes the nickel sheet with openings used in evaporation and photolithography, typically 15–200μm thick. It does not form an image by itself. It blocks or passes light and vapour according to the opening shape. Once opening line width reaches 20–50μm, whether the edges are straight, whether burrs are present and whether the sheet lies flat decide how clean the deposited film turns out. Unlike a stencil, the mask is often carried on a glass or silicon substrate, so accuracy hangs on two lines, exposure and electroforming. Double-sided alignment at ±5μm and LDI resolution at 8μm/8μm are largely settled at development. For customers in Tianjin and nearby, the drawing puts line width and flatness first.
Three failures cluster at the opening edge. Line narrowing comes first: after development, resist residue eats a few microns off a fine rib, the flash tester reads 17μm where 20μm was called for, and the evaporated line follows. Burrs come from current density at 1–4 A/dm² run without staging. Field lines crowd at the corners, nickel grows an extra rim there, and the rim scratches the substrate once the mask is clamped. Warpage follows a release with stress still locked in; flatness drifts from 0.02mm to 0.08mm, vacuum chuck cannot pull the sheet flat, and film thickness varies across it. Downstream work cannot repair any of these. Tianjin electroformed mask plate processing has to hold the stretch from exposure to release. The 0.02–0.08mm band is a measured range across batches, not a promise.
Parameter Window
• Opening line width sits mainly at 20–50μm, with LDI resolution 8μm/8μm and line deviation held inside ±2μm; points are taken at edge, centre and corner.
• Mask thickness is graded 15–200μm, flatness sampled by batch at 0.02–0.08mm, and an out-of-band sheet does not move on.
• Double-sided alignment ±5μm and hole position accuracy ±7μm are scanned before and after exposure; a shifted coordinate sends the sheet back.
• Minimum opening ≥25μm, pitch ≥120μm and hole spacing ≥50μm; the 20μm rib gets its own exposure compensation.
• Nickel-cobalt hardness 450–550HV and wall roughness ≤0.01μm are weighed together with internal stress rather than chased upward.
• Measurement at 23±2℃ with Cpk≥1.33 in the first month; the report names the gauge and the sample points, and both line width and flatness follow that report.
Manufacturing Process (8 Steps)
1. Drawing intake — record opening line width, pitch, thickness and substrate material. Drawings from Tianjin customers often list line width and flatness separately; a missing field gets asked about.
2. Substrate prep — glass or silicon is cleaned, degreased and dried, and its own flatness is measured before anything else; dust means another wash.
3. Conductive layer — a seed layer is deposited and sheet resistance checked per piece; a corner left uncovered is redone, not patched later.
4. Film and exposure — resist is laminated and LDI writes the pattern at 8μm/8μm, with double-sided alignment ±5μm set as the datum.
5. Development — fine ribs and micro holes are flushed clean, residue is checked against the seed layer, and line width gets a first scan here.
6. Electroforming — current density 1–4 A/dm² is raised in stages up to 15–200μm, with edge-to-centre thickness watched during the run.
7. Release and anneal — the nickel mask is peeled from the low-stress corner of the carrier, then annealed at low temperature; the order does not reverse.
8. Final check — an imaging system and flash tester scan line width, position and flatness, burrs are judged under a microscope, and the card travels with the goods.
Core Advantages
1. Line width has a basis — Tianjin electroformed mask plate processing ties LDI resolution 8μm/8μm to a post-development scan, so a 20μm rib is not left to guesswork.
2. Fewer corner burrs — staged current stops extra nickel piling up at the corners; the opening edge stays clean and does not scrape the substrate in the fixture.
3. Flatness is accounted for — low-temperature annealing after release lets stress go, and 0.02–0.08mm is logged per batch so vacuum contact has a number.
4. Alignment holds — ±5μm double-sided alignment is scanned on both sides of exposure, and a shifted sheet is picked out before it reaches evaporation.
5. Reports can be traced — line width, flatness, sample points and temperature are kept for each sheet, so a dispute resolves down to one piece.
6. One wording throughout — customers in Tianjin and nearby hear the measured value from the report, not a spoken promise of an extreme figure.
Typical Applications
• Evaporation masks: thin nickel sheet, opening line width 20–50μm, grown whole on a glass carrier
• Aperture and slit blades: rib width 20μm, where edge burrs show up directly as stray light
• Encoder discs: track 50μm±0.5μm, with double-sided alignment ±5μm setting line consistency
• Mini/Micro LED transfer masks: substrate up to 610×660mm, edge and centre flatness controlled together
• Micro-hole mesh masks: hole tolerance ±3μm, the micro-hole area cleared at development
• Export parts: RoHS and inspection report shipped along, with line width and flatness accepted against the report
Design and Selection Notes
1. Fix opening line width and pitch before talking thickness. Change either number and exposure compensation plus current staging both need rework.
2. Narrower is not automatically better. Ribs below 20μm on 15–200μm stock can collapse at development, so a sample run comes before the drawing is signed.
3. Settle the carrier material early. Glass and silicon take different pre-treatments and release methods; finding out at release is too late.
4. Discuss flatness against measured values. The 0.02–0.08mm band is a range; if a batch drifts past 0.05mm, go back to the anneal step and remeasure.
5. If line width drifts past ±2μm after development, return to LDI and development for a recheck rather than trimming the edge downstream.
6. Read thickness and hardness together. The 450–550HV window is a range, and pushing hardness up raises internal stress, which makes flatness harder to keep.
7. Keep the three sets of figures for line width, flatness and burrs, so a Tianjin customer can pull the record for that sheet on a later visit.
On the floor, Tianjin electroformed mask plate processing is three things holding at once: opening line width, whole-sheet flatness and edge burrs. Line width rests on LDI resolution 8μm/8μm plus the development scan, flatness on annealing after release and sampling at 23±2℃, and burrs on staged current and a microscope call. All three go into the inspection report, and an out-of-band sheet is rejected rather than covered by a spoken number. One batch of 20μm ribs measured 17μm after development; the cause was residue left in the flush, and the exposure had to be run again. For an order with firm line width and flatness targets, fixing the gauge, sample points and acceptance wording at the sample stage costs less than sorting finished sheets.