Edge roughness of an electroformed disc track describes how ragged the light-transmitting edge of that track actually is: take the absolute profile deviation over the evaluation length, average it arithmetically, and you get Ra in μm. It measures height variation along the edge profile, which is a different account from sidewall angle. A white-light interferometer with a 20× objective traces the full circumference at a 0.25 mm sampling length and a 1.25 mm evaluation length, reporting Ra, Rz and Rmax together. Two discs at 0.03 μm and 0.10 μm look identical under a lamp and produce two different waveforms once installed. The rougher the edge, the more light scatters, and the further the effective aperture boundary wanders.
Out-of-spec edge roughness on a production line usually shows up as one of three symptoms. The first is flux ripple beyond ±1.2%: the envelope of the full-revolution waveform shivers on the scope, and the same disc reads differently when mounted at another angle. The second is duty cycle drift, where a track designed at 1:1 measures 53:47 and no threshold adjustment pulls it back. The third is rising jitter, with phase error on an incremental encoder creeping from 0.02° to 0.08° at low speed, which the servo feels as stick-slip. All three trace back to one place: edge Ra pushed past 0.09 μm, with scatter consuming 0.4–0.8 μm of effective aperture. When two inspectors measure with different sampling lengths, their Ra values can differ by 0.01 μm, and the argument over rework versus scrap starts there.
Parameter Window
• Ra accept line at 0.02–0.06 μm, eight sectors per disc, any sector past 0.08 μm goes to rework.
• Sampling length 0.25 mm and evaluation length 1.25 mm are written into the inspection card; change the instrument, not the convention.
• Track width 50 μm ±0.5 μm at a 1:1 duty cycle, with edge burrs held separately to Rmax ≤0.4 μm.
• Full-revolution flux ripple ≤±1.2%, single-edge position uncertainty kept inside 0.3 μm.
• Nickel deposit 25–60 μm at 1–4 A/dm², with the outer band dropped another 0.5 A/dm² to slow growth.
• Low-temperature anneal at 120–150 °C for 2 h, Ra shift ≤0.005 μm before release.
Manufacturing Process (8 Steps)
1. Substrate cleaning — stainless substrate degreased, acid dipped and rinsed until surface particles sit at the 0.1 μm level.
2. Coating and exposure — LDI writes the tracks at 8 μm/8 μm resolution, double-sided alignment ±5 μm, edge features biased by 0.5 μm.
3. Development — time set per resist thickness, edges cleared without collapse, undercut held within 0.3 μm.
4. Resist inspection — an image measurer checks track edge straightness and notches, and ragged parts never reach the bath.
5. Electroforming — current density staged across 1–4 A/dm², starting at 0.5 A/dm², one step lower at the edge zone than at centre.
6. Stripping — the nickel sheet lifts from a substrate corner at a shallow angle, never pried, so the edge is not torn into burrs.
7. Annealing — 2 h at 120–150 °C relaxes deposition stress so the edge stops springing back.
8. Edge re-measurement — the interferometer walks the full circumference for Ra and Rz, the flux bench records ripple, and a report is issued.
Core Advantages
1. Holding electroformed disc track edge roughness inside 0.06 μm brings full-revolution flux ripple from ±1.5% down under ±1.0%.
2. Sector-to-sector consistency is held by the process card, with Ra range ≤0.015 μm across eight sectors, so remounting does not produce a second waveform.
3. With scatter suppressed, duty cycle distortion falls from 3% to 0.8% and decoding margin opens up.
4. Annealing runs before final measurement, so a disc that sits two days at the customer does not curl its edge again.
5. A fixed measurement convention lets Ra data from two plants sit in one table, which leaves less room for dispute.
6. One current-staging table covers a whole batch from the same bath, so a changeover only needs the first disc rechecked.
Typical Applications
1. Metal code discs for incremental encoders, where A/B duty cycle and phase error both ride on the edge.
2. Multi-track absolute discs, whose narrowest slits at 20 μm suffer most from edge burrs.
3. Rotary and linear gratings, where edge Ra converts directly into moiré fringe signal-to-noise.
4. Entrance slit blades for spectrometers, since a burred slit mouth feeds stray light to the detector.
5. Aperture blades in laser scanners, where edge scatter is one source of spot trailing.
6. Export discs requiring RoHS documentation and a full-revolution inspection report shipped with the goods.
Design and Selection Notes
1. Set the flux ripple target first, then work back to an Ra ceiling; the reverse order tends to produce a hollow spec.
2. Lower edge Ra is not automatically better. Below 0.02 μm there is almost no gain in signal-to-noise, while cost steps up a tier.
3. Narrower tracks give the edge a larger share of the width, so slits under 20 μm need their own bias instead of inheriting wide-slit experience.
4. If Ra drifts more than 0.01 μm after annealing, go back to the bath and check current staging and additive balance.
5. Instrument model and sampling length belong on the drawing together with Ra; an Ra number without a convention is not a spec.
6. On parts held to ±5 μm double-sided alignment, measure edge and track centre together rather than picking one.
7. For prototypes, run the full-revolution flux bench before chasing single-point Ra; it exposes problems faster.
Treating electroformed disc track edge roughness as a measurable quantity beats asking for a smooth edge in general terms. Between 0.02 and 0.06 μm the scatter loss is negligible and both flux ripple and duty cycle distortion stay within what the circuit can correct; past 0.10 μm, threshold trimming only hides the symptom. The order of diagnosis on the floor is simple: full-revolution waveform first, then Ra range across eight sectors, and only then the interferometer to locate the rough stretch. For orders with a hard track Ra re-measurement requirement, freeze sampling length, evaluation length and sector count at the prototype stage and run production against that card; when a customer sends only the words 'edge must be smooth', ask which instrument and which convention before quoting any Ra figure.
Contact:赖先生
Phone:+86 18938693450
Tel:0755-2708-8292
Email:yw9@zldsmt.com
Add:深圳市宝安区福永镇新和村福园一路华发工业园A3栋