Foshan electroformed mesh processing is about whether a screen hole array is orderly: at the same mesh count, are all holes the same size, does hole spacing hold, and do the mesh counts read from different zones of the web agree? A screen is neither punched nor etched; the hole is set by the developed resist sidewall and the nickel growth front together, so a little more undercut or a little current crowding at the rim quietly rewrites the shape. On receiving a finished web, the inspector takes upper, middle and lower zones on a vision gauge to measure aperture and spacing, then converts mesh count from holes per unit length; an out-of-tolerance piece is tagged on the spot for rework or scrap. With meshes down to 15 μm and holes to 25 μm, a few microns of deviation turn straight into a wrong cut point in particle grading.
Three routes make the mesh count go off on the line. Development undercut eats down the resist sidewall, the mouth opens wider while the bottom keeps its size, and the hole becomes a cone wider at the top; dense zones join in strings, and a flash gauge reads one zone low on the spot. Rim nodule growth is another: at a current density of 1–4 A/dm² the field lines crowd at the corners, nickel grows faster along the resist edge than in the middle, a ring bulges at the mouth, aperture ±3 μm cannot hold. The third is lift-off damage: when the nickel web is raised in one sheet under uneven load, round holes are dragged into ovals, neighbours skew together, and the ≥50 μm spacing layout falls out of order. What Foshan electroformed mesh processing has to watch is the hole-shape account between development and lift-off.
Parameter Window
• Mesh count deviation reported as a measured range: back-calculate holes per unit length from pitch ≥120 μm and hole spacing ≥50 μm, log zone-by-zone readings on the inspection card, and promise no absolute mesh count figure.
• Minimum opening ≥25 μm and aperture tolerance ±3 μm, micro-hole meshes held to the same band; a vision gauge samples zone by zone, and out-of-tolerance apertures never reach the next step.
• Mesh thickness banded 15–200 μm, thin meshes with little undercut allowance getting a shorter development time, and wall roughness ≤0.01 μm written into the inspection card as well.
• Hole position accuracy ±7 μm and roundness ±0.002 mm, round holes re-measured by quadrant, never released on a single diameter reading.
• Current density staged at 1–4 A/dm², the hole-rim zone dropped one band to suppress nodules, nickel-cobalt alloy hardness 450–550 Hv.
• Tension 10–55 N (±1 N internal) re-measured after framing, with web flatness against mesh count checked once more after the AB-glue frame is fitted.
Manufacturing Process (8 Steps)
1. Substrate prep — cut the stainless substrate, degrease, clean and dry, and let it rest to temperature before dry-film lamination.
2. Lamination and exposure — write the hole array by LDI after lamination at 8 μm/8 μm resolution, mesh count placed from the back-calculated pitch.
3. Development — developer temperature and time held to the thickness band, fine-hole sidewalls flushed clean of residue so undercut narrows with it.
4. Resist check — a vision gauge samples hole mouths and sidewall slope; cone holes and collapsed edges are stopped on the spot before the bath.
5. Electroforming — current density staged at 1–4 A/dm², the rim dropped a band to curb edge effects, grown to target thickness.
6. Lift-off — raise the nickel web in one sheet from a low-stress corner at a shallow angle, dense zones backed first.
7. Low-temperature anneal — relieve internal stress in the nickel so web flatness settles and mesh count no longer drifts with spring-back.
8. Final recheck — vision and flash gauges scan aperture ±3 μm and hole position ±7 μm zone by zone, then issue the inspection report.
Core Advantages
1. Even array — Foshan electroformed mesh processing locks undercut and current edge into one window, so mesh count readings line up across several zones of one web.
2. Traceable count — mesh count deviation given as a measured range, the inspection card shipping with the goods so a customer calibration can be reused.
3. Held aperture — aperture ±3 μm reads the same after lift-off and anneal, without the substrate propping it round.
4. Clean rims — current stepped down cuts nodules and burrs, so a flash gauge finds far fewer burred hole outlines.
5. Steady lots — a dozen screens from one bath share a compensation card, dense-zone spread stays small, lot changes need no re-tune.
6. Clear delivery terms — for Foshan and nearby customers, drawing requirements and the inspection report use one set of terms, so communication stays direct.
Typical Applications
1. Ceramic powder and building-material screening meshes, where mesh count sets the cut point of particle grading.
2. Precision filtration nickel meshes, where micro-hole aperture tolerance ±3 μm decides retention accuracy.
3. Paste filtration screens and printing mesh plates, where rim nodules scratch the web face and blind the screen.
4. Acoustic dust meshes and sensor vent meshes, where ≥50 μm hole spacing needs an orderly layout.
5. Abrasive and semiconductor material grading screens, where distorted hole shape skews particle-size calls.
6. Export screens needing RoHS and traceable reports, the hole-shape inspection card shipping with the goods.
Design and Selection Notes
1. Back-calculate mesh count from pitch and hole spacing first; do not order on a mesh number alone, state aperture and pitch as well.
2. Put development time and bath temperature into the process card; shorten thin meshes separately since their undercut allowance is thin to begin with.
3. Step rim current density down one band, do not sit at the 4 A/dm² ceiling for long runs growing nodules.
4. Start the lift at a low-stress corner and back dense zones first, do not leave a few holes to take the load alone.
5. Put low-temperature anneal after lift-off; reverse the order and stress will pull the hole shape out of round.
6. Re-measure roundness by quadrant, since a single diameter reading easily lets an oval hole through.
7. Report mesh count deviation as a measured range with no absolute precision promise; if a zone drifts beyond the card range, return to the development and exposure stages for a recheck.
Taken apart, Foshan electroformed mesh processing is not about the place name but about the account from resist image to finished web on aperture uniformity and mesh count. The resist sets the array, development sets sidewall slope, current sets how the rim grows, and lift-off sets whether the hole is dragged out of round; loosen any one and aperture ±3 μm and roundness ±0.002 mm are just figures on paper. What separates capable lines is whether the mesh counts still line up across a dozen screens from one bath and after a fresh lot of dry film, not whether a few handsome holes can be picked from a single piece. A thinner web is not always better: thin meshes have little undercut allowance and ask more of development and lift-off. For screening and filtration orders from Foshan and nearby customers, fix the compensation value, development time, current bands and lift angle into the process card at sampling stage and run to that card in volume, far cheaper than sorting piece by piece on a vision gauge afterwards.
Contact:赖先生
Phone:+86 18938693450
Tel:0755-2708-8292
Email:yw9@zldsmt.com
Add:深圳市宝安区福永镇新和村福园一路华发工业园A3栋