Guangzhou electroformed stencil processing makes the nickel stencil with apertures used on SMT printing lines, generally 15–200μm thick. Paste reaches the pads through those apertures. Aperture consistency describes how far the size, position and walls of thousands of holes on one stencil scatter, not how good a single hole looks. On one board, a ±3μm aperture difference can move paste volume enough to leave cold joints or bridges after reflow. Frame tension at 10–55N decides whether the mesh lies flat against the board under the squeegee. For customers in Guangzhou and nearby working in electronics and SMT, the drawing puts aperture size, step height and tension first.
Three problems turn up on the line. Aperture drift comes first: an automatic stencil inspection machine scans one nominal hole and finds 4μm between the corner and the centre, then the paste thickness gauge reports uneven volume and the fine-pitch pads fail first. Step transition collapse follows: at a 0.02–0.08mm step the aperture near the boundary is pulled out of shape, one side gets more paste than the other, and bridging appears after reflow. Tension loss comes third: the frame reads inside 10–55N at intake, drops below the lower limit after a few hundred prints, the mesh sags under the squeegee and the aperture shifts out of position. None of these is recovered by tuning the printer. Guangzhou electroformed stencil processing has to hold the stretch from apertures through steps to tension.
Parameter Window
• Stencil thickness is graded 15–200μm, aperture tolerance ±3μm and hole position accuracy ±7μm, with on-board scatter tracked per batch.
• Minimum opening ≥25μm, pitch ≥120μm and hole spacing ≥50μm; fine-pitch apertures are trimmed individually.
• Frame tension runs 10–55N with an internal control of ±1N, measured before and after the machine, and a stencil below the limit is re-tensioned.
• Step height sits at 0.02–0.08mm, the transition slope follows the drawing, and apertures at the boundary are measured on their own.
• Wall roughness ≤0.01μm and nickel-cobalt hardness 450–550HV, with print life sampled across 15000 cycles.
• Scanning at 23±2℃ on an automatic stencil inspection machine with Cpk≥1.33; aperture consistency follows the measured report.
Manufacturing Process (8 Steps)
1. Drawing intake — record thickness, apertures, steps and frame size. Drawings from Guangzhou SMT customers often list apertures and tension apart; a missing field gets asked about.
2. Mandrel prep — the substrate is cleaned, degreased and dried, and its flatness measured first; any dust means another wash.
3. Conductive layer — a seed layer is deposited and sheet resistance checked per piece; a corner left uncovered is redone.
4. Film and exposure — resist is laminated and LDI writes the pattern at 8μm/8μm, with double-sided alignment ±5μm set as the datum.
5. Development — apertures are flushed clean, residue is checked against the seed layer, and hole size gets a first scan here.
6. Electroforming — current density 1–4 A/dm² rises in stages up to 15–200μm, with edge-to-centre thickness watched during the run.
7. Release and steps — the nickel sheet is peeled whole from the mandrel, locally thinned to form steps, then annealed at low temperature.
8. Final check — an automatic inspection machine scans apertures and position, a gauge reads tension at 10–55N and an imaging system checks the steps; the report travels with the goods.
Core Advantages
1. Apertures stay uniform — Guangzhou electroformed stencil processing ties LDI resolution 8μm/8μm to a post-development hole scan, so ±3μm is counted across the board rather than picked hole by hole.
2. Position holds — hole position accuracy ±7μm is scanned before and after exposure, and a shifted stencil is picked out on the spot.
3. Steps do not collapse — the 0.02–0.08mm transition is trimmed on its own, keeping the boundary aperture square so paste splits evenly.
4. Tension can be traced — 10–55N is logged before and after the machine within ±1N, and a stencil that drops is re-tensioned rather than forced through.
5. Life has a number — walls and apertures are sampled over 15000 print cycles, and wear trends are kept instead of guessed.
6. Reports land — customers in Guangzhou and nearby hear the measured figure from the report, not a spoken promise of an extreme figure.
Typical Applications
• Phone motherboard stencils: 0.1–0.2mm thick, fine-pitch at ≥120μm
• Automotive control boards: apertures at ±3μm, sampled over 15000 prints
• Server and communication boards: large stencils with many apertures, tension held at 10–55N
• Step stencils: local thinning of 0.02–0.08mm to serve fine leads and large pads together
• QFN and BGA fine-pitch parts: minimum opening ≥25μm, wall roughness ≤0.01μm
• Export parts: RoHS and inspection report shipped along, apertures and tension accepted against the report
Design and Selection Notes
1. Fix aperture size and thickness before discussing tension. Change either number and exposure compensation plus the tensioning method both need rework.
2. Higher tension is not automatically better. Past the 55N ceiling the frame carries more internal stress and deforms more readily under load.
3. Set step height from the pad difference. The 0.02–0.08mm band is a range, and cutting it deeper for its own sake pulls the transition out of shape.
4. Confirm that a ≥25μm opening can actually be measured, and settle pitch at ≥120μm, before the drawing is signed.
5. If apertures on one stencil drift past ±3μm, return to LDI and development for a recheck rather than trimming at the back end.
6. Measure tension before and after the machine; if it drops past the ±1N internal control, re-tension instead of letting sag pull alignment off.
7. Keep the three sets of figures for apertures, steps and tension so a Guangzhou customer can pull the stencil record on a later visit.
On the floor, Guangzhou electroformed stencil processing is three things holding at once: aperture size, step transition and frame tension. Apertures rest on LDI resolution 8μm/8μm plus the post-development scan, steps on local thinning and an imaging check, and tension on two readings around the press. All three go into the report, and an out-of-band stencil is rejected rather than covered by a spoken figure. One 0.15mm stencil showed corner apertures 4μm larger than the centre; the cause was uneven development flushing, and the development had to be run again. For an order with a firm aperture consistency target, fixing the gauge, sample points and acceptance wording at the sample stage costs less than sorting finished stencils.